Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Nilit
Trade Name Nilitop
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used for applications that need a high dimensional stability, like automotive connectors, transmission housings for electro motors or parts that are subjected to high UV radiation, like exterior automotive parts.Key characteristics: Good overall mechanical performanceLow moisture absorptionGood UV resistanceGood thermal performanceInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792, ISO 1183
Water Absorption 0.10 %
0.10 %
23°C, 24h in H<sub>2</sub>O; sim. ISO 62
Water Absorption at Saturation 0.40 %
0.40 %
sim. ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Euronil
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Euronil
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ISO 527, ASTM D638
Elongation at Break 2.5 %
2.5 %
ISO 527, ASTM D638
Flexural Yield Strength 210 MPa
30500 psi
ISO 178, ASTM D790
120 MPa

@Temperature 90.0 °C
17400 psi

@Temperature 194 °F
ISO 178, ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178, ASTM D790
4.80 GPa

@Temperature 90.0 °C
696 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75, ASTM D648
Vicat Softening Point 213 °C
415 °F
49 N; ISO 306, ASTM D1525
222 °C
432 °F
9.8 N; ISO 306, ASTM D1525
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Oxygen Index 20 %
20 %
ASTM D2863
Glow Wire Test 750 °C

@Thickness 0.800 mm
1380 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
750 °C

@Thickness 3.20 mm
1380 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Electrical Properties Metric English Comments
Dielectric Strength 23.0 kV/mm

@Thickness 2.00 mm
584 kV/in

@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index 175 V

@Thickness 3.20 mm
175 V

@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
400 V

@Thickness 3.20 mm
400 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Descriptive Properties Value Comments
Heat Resistance - Ball Test OK
at 125°C, IEC 309
OK
at 165°C, IEC 309
Copyright © lookpolymers.com All Rights Reserved