| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 4.50 J/cm² - NB | 21.4 ft-lb/in² - NB | Average value: 9.06 J/cm² Grade Count:71 |
| Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
| Charpy Impact Unnotched | 4.50 - 999.9 J/cm² @Temperature -30.0 - 30.0 °C |
21.4 - 4759 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 9.28 J/cm² Grade Count:42 |
| Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 19-7652 Polyamide 46, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Reduced moment of inertia comp.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | flatwise; ISO 179 1fU |
| Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 20-7908 Polyphthalamide, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | flatwise; ISO 179 1fU |
| Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Grupo Repol Dinalon® B1X25 G30W PA6 30% Glass Fiber, Reduced Water Abs. Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
| LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | flatwise; ISO 179 1fU |
| Lehmann & Voss PLASLUBE NY-1/TF/20/BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
| LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
| LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced EMI shielding product based on Polycarbonate (PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
| Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
| EMS-Grivory Grivory® HT2V-3H LF PA*-GF30 Grivory TH2V-3H LF is a glass fiber reinforced (30%), PTFE modified engineering thermoplastic based on semi-crystalline partially aromatic copolyamide. Polymer designation acc. ISO: PA6T/66 Polymer .. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30 Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid.. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/IeU |
| Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/IeU |
| Addiplast Addinyl B2 G30 Nylon 6, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||