Polymer Property : Charpy Impact Unnotched = 4.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -40.0 °C
19.0 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 KV30 Nylon 6 for injection molding, 30% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Charpy Impact Unnotched 4.00 J/cm² - NB

@Temperature -30.0 - -20.0 °C
19.0 ft-lb/in² - NB

@Temperature -22.0 - -4.00 °F
Average value: 4.13 J/cm² Grade Count:9
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact Unnotched 4.00 J/cm² - NB

@Temperature -40.0 - -20.0 °C
19.0 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 10.9 J/cm² Grade Count:98
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1-7984 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® PC-50/GF/30/TF/15/ BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced
Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Arnite® TV4 244 S PBT-GF20 FR
20% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179-1eU
Barlog Plastics KEBATRON C1040G5 PPS, cross-linked, 40% glass fiber reinforced
PPS-GF40Information provided by BARLOG plastics GmbH.
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced
General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected ..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced
Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).Data was collected by IS..
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry)
Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179 eU
Radici Radiflam® B RV 300 AE Polybutylene Terephthalate
Raditer® B RV 300AE is a glass fiber reinforced, self-extinguishing UL-94 V-0 (with halogen) thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent therma..
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
LATI Latiohm 75/4-03 PD01 G/20 PBT, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..