| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | Nilit (formerly Frisetta Polymer) |
| Trade Name | FRIANYL |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nilit FRIANYL A63 GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
| Water Absorption | 1.4 - 2.1 % | 1.4 - 2.1 % | ISO 62 |
| Water Absorption at Saturation | 6.0 - 8.0 % | 6.0 - 8.0 % | ISO 62 |
| Viscosity Measurement | 145 | 145 | Viscosity index; ISO 307 |
| Linear Mold Shrinkage | 0.0040 - 0.012 cm/cm | 0.0040 - 0.012 in/in | FRISETTA Test Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 179 MPa | 26000 psi | ISO 2039-1 |
| Tensile Strength at Break | 180 MPa | 26100 psi | ISO 527 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527 |
| Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
| Flexural Strength | 240 MPa | 34800 psi | ISO 178 |
| Flexural Modulus | 8.00 GPa | 1160 ksi | ISO 178 |
| Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | DIN 53453 |
| NB | NB | ISO 179/1eU | |
| 4.50 J/cm² <br>@Temperature -40.0 °C |
21.4 ft-lb/in² <br>@Temperature -40.0 °F |
DIN 53453 | |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | DIN 53453 |
| 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
| Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous; FRISETTA Test Method |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ISO 75 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
| Dissipation Factor | 0.020 <br>@Frequency 1e+6 Hz |
0.020 <br>@Frequency 1e+6 Hz |
IEC 250 |
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |