Momentive Performance Materials FRV1106 Red Fluorosilicone Adhesive Sealant, Fuel Resistant Paste

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials FRV1106 Red Fluorosilicone Adhesive Sealant, Fuel Resistant Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part acetoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: For use in contact with fuel, solvents, and chemicals.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength, Ultimate 3.33 MPa
483 psi
Elongation at Break 230 %
230 %
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Continuous useful temperature.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Dielectric Constant 6.3

@Frequency 1000 Hz
6.3

@Frequency 1000 Hz
Dielectric Strength 13.7 kV/mm
348 kV/in
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F