Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C

@Load 5.001 kg
203 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs S20 ABS
Information provided by Polykemi AB
Vicat Softening Point 95.0 °C

@Load 5.001 kg
203 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYasa 2008F UV-stabilized, High Flow ASA
Information provided by Polykemi AB
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa HC-110 Modified ABS
Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 95.0 °C

@Load 1.00 kg
203 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C/hour; ISO 306
Ineos ABS Lustran® M210TF ABS Pellets
Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo..
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C/hour; ISO 306
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Vicat Softening Point 95.0 °C

@Load 1.00 kg
203 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa FRABS-518 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution PS 147F GPPS
Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro..
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
ISO 306
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 95.0 °C

@Load 0.999 kg
203 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro..
Vicat Softening Point 95.0 °C

@Load 5.10 kg
203 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3000 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-..
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibilac® PW-957 ASA Polymer
Injection
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibilac® PW-997S ASA Polymer
Extrusion
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-709 ABS
Super impact
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
High impact; high gloss
Vicat Softening Point 95.0 °C

@Load 0.999 kg
203 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 1012 Polystyrene
General purpose polystyreneHigh impact resistance, good melt flow rate, good flexibilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 95.0 °C

@Load 1.00 kg
203 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibiton® PB-5925 SBC
Transparency, high stiffness, injection grade
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756S ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-33 Polystyrene
Standard grade
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
Vicat Softening Point 95.0 °C

@Load 1.00 kg
203 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant
High Flow
Copyright © lookpolymers.com All Rights Reserved