| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 98.0 °C @Load 5.001 kg |
208 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYabs SS0 GK10 ABS, High Flow Information provided by Polykemi AB |
|||
| Vicat Softening Point | 98.0 °C @Load 1.00 kg |
208 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
| Vicat Softening Point | 98.0 °C @Load 5.001 kg |
208 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
| Vicat Softening Point | 98.0 °C @Load 5.10 kg |
208 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
| Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
| Vicat Softening Point | 98.0 °C @Load 5.10 kg |
208 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
| Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
| Vicat Softening Point | 98.0 °C @Load 5.10 kg |
208 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Styrolution Luran® S 767KE ASA Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos.. |
|||
| Vicat Softening Point | 98.0 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
| Vicat Softening Point | 98.0 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
| Vicat Softening Point | 98.0 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
| Vicat Softening Point | 98.0 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 98.0 °C @Load 0.999 kg |
208 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASTIR HI 0412 Polystyrene Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 98.0 °C @Load 0.999 kg |
208 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASTIR HI 0810 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, high impact resistance, good melt flow rate, good light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-717C ABS Medium impact |
|||
| Vicat Softening Point | 98.0 °C @Load 1.00 kg |
208 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747S ABS - Extrusion High Impact Extrusion |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-758 ABS - Transparent Transparent |
|||
| Vicat Softening Point | 98.0 °C @Load 1.00 kg |
208 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
| Vicat Softening Point | 98.0 °C @Load 5.001 kg |
208 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746Y ABS
(discontinued **) Medium flow, high impact |
|||
| Vicat Softening Point | 98.0 °C @Load 5.00 kg |
208 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746Y ABS
(discontinued **) Medium flow, high impact |
|||