| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 30 - 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 - 40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
| NIZHNEKAMSKNEFTEKHIM PP 1452S (H39S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
| Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 190 °C |
30 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition G; ASTM D1238 |
| Global ST-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | ASTM D1238 |
| Kolon Kocetal® VT701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
| Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Kotec Carbotex K-20MRA30 Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesIn.. |
|||
| Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
nozzle diam 2.095 mm; ISO 1133 |
| Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | ASTM D 1238 |
| Karina 1000/40451-IE MBPEB White Color Concentrate Filled white color concentrate recommended for polyolefin application according to the Mercosul Regulation (Resoluçao 105). This products meets the FDA Regulation.Information provided by Karina I.. |
|||
| Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 250 °C |
30 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
| LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
| Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 380 °C |
30 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
| Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 265 °C |
30 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
| SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
| Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 250 °C |
30 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
| Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 250 °C |
30 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Melt Flow | 30 g/10 min @Temperature 190 °C |
30 g/10 min @Temperature 374 °F |
ASTM D1238 |
| Sanyo PELESTAT® 300 Antistatic Additive PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a var.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | ASTM D1238 |
| Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow 20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
| Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 200 °C |
30 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
| Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | ASTM D1238 |
| A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 260 °C |
30 g/10 min @Load 11.0 lb, Temperature 500 °F |
estimated from MVR using room temperature density; ISO 1133 |
| Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | ASTM D1238 |
| ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5070 is an ethylene acrylic acid copolymer characterized by high melt index and 9% acrylic acid comonomer content. Escor 5070 combines easily processing and adhesion to po.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
| EMS-Grivory Grivory® CR 9 HV PA* Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr.. |
|||
| Melt Flow | 30 g/10 min | 30 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
| EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| ExxonMobil Exxtral™ LNV 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high gloss, low warpage, and low discoloration in contact with hot water/steam in large electrical appliance such as washing mach.. |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg |
30 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7. |
| Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
| Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
| Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
| Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Phillips 66 COPYLENE® CR300CL-01 Polypropylene Random Copolymer COPYLENE® CR300CL-01 is a reactor grade, clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with anti-stat for excellent mold re.. |
|||
| Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
ASTM D1238 |
| A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 30 - 50 g/10 min @Load 21.6 kg, Temperature 170 °C |
30 - 50 g/10 min @Load 47.6 lb, Temperature 338 °F |
DDIN 53.735 |
| Lubrizol Advanced Materials Pearlbond® 118 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |
|||