Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low SlipApplications:Food Packaging, Case Shrink Wrap, LaminationsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.210 GPa
30.5 ksi
ASTM D882
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Coefficient of Friction 0.50
0.50
ASTM D1894
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 4.5 %
4.5 %
ASTM D2457
Gloss 75 %
75 %
at 45°. ASTM D 2457
120 %
120 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F