EMS-Grivory Grivory® XE 4073 nat PA610

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4073 nat PA610.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materials and its eco-profile is very favorable when compared to similar products based on crude oil. The main features of Grilamid XE 4073 are:Low water absorptionGood fatigue resistanceGood heat, UV and chemical resistanceEasy processingBased to 62% on renewable resources Grilamid XE 4073 natural is particularly suitable for the manufacturing of technical injection molded parts in the application fields of:AutomotiveMechanical engineeringSports & leisure goodsDomestic applianceInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 3.5 %
3.5 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 82.0 MPa
11900 psi
conditioned; ISO 2039-1
128 MPa
18600 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
65.0 MPa
9430 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
2.20 GPa
319 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
dry; ISO 179/1eA
1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 130 °C
212 - 266 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
35.0 kV/mm
889 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Release agent
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Connectors
Electrical appliances
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Calandering
Film Extrusion
Injection Molding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Product Attributes Bio based Polyamide
Special Characteristics Light stabilized or stable to light