Category | Polymer , Thermoplastic , Nylon , Nylon 46 |
Manufacturer | DSM Engineering Plastics |
Trade Name | Stanyl® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | DSM Stanyl® TW341-J PA46.pdf |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ | dry; ISO 1183 |
Moisture Absorption | 3.70 % | 3.70 % | Sim. To ISO 62 |
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.0 MPa | 7980 psi | cond; ISO 527-1/-2 |
100 MPa | 14500 psi | dry; ISO 527-1/-2 | |
30.0 MPa @Temperature 200 °C |
4350 psi @Temperature 392 °F |
ISO 527-1/-2 | |
35.0 MPa @Temperature 180 °C |
5080 psi @Temperature 356 °F |
ISO 527-1/-2 | |
40.0 MPa @Temperature 160 °C |
5800 psi @Temperature 320 °F |
ISO 527-1/-2 | |
50.0 MPa @Temperature 120 °C |
7250 psi @Temperature 248 °F |
ISO 527-1/-2 | |
Elongation at Break | 40 % | 40 % | dry; ISO 527-1/-2 |
>= 50 % | >= 50 % | cond; ISO 527-1/-2 | |
>= 50 % @Temperature 120 °C |
>= 50 % @Temperature 248 °F |
ISO 527-1/-2 | |
>= 50 % @Temperature 160 °C |
>= 50 % @Temperature 320 °F |
ISO 527-1/-2 | |
>= 50 % @Temperature 180 °C |
>= 50 % @Temperature 356 °F |
ISO 527-1/-2 | |
>= 50 % @Temperature 200 °C |
>= 50 % @Temperature 392 °F |
ISO 527-1/-2 | |
Tensile Modulus | 1.00 GPa | 145 ksi | cond; ISO 527-1/-2 |
3.30 GPa | 479 ksi | dry; ISO 527-1/-2 | |
0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 | |
0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 | |
0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 | |
8.00 GPa @Temperature 120 °C |
1160 ksi @Temperature 248 °F |
ISO 527-1/-2 | |
Flexural Modulus | 0.900 GPa | 131 ksi | cond; ISO 178 |
3.00 GPa | 435 ksi | dry; ISO 178 | |
0.600 GPa @Temperature 160 °C |
87.0 ksi @Temperature 320 °F |
ISO 178 | |
0.800 GPa @Temperature 120 °C |
116 ksi @Temperature 248 °F |
ISO 178 | |
Fatigue Strength | 12.0 MPa @# of Cycles 1.00e+8 , Temperature 140 °C |
1740 psi @# of Cycles 1.00e+8 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
21.0 MPa @# of Cycles 1.00e+7 , Temperature 140 °C |
3050 psi @# of Cycles 1.00e+7 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
30.0 MPa @# of Cycles 1.00e+6 , Temperature 140 °C |
4350 psi @# of Cycles 1.00e+6 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
35.0 MPa @# of Cycles 100000 , Temperature 140 °C |
5080 psi @# of Cycles 100000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
37.0 MPa @# of Cycles 10000 , Temperature 140 °C |
5370 psi @# of Cycles 10000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
39.0 MPa @# of Cycles 1000 , Temperature 140 °C |
5660 psi @# of Cycles 1000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
41.0 MPa @# of Cycles 100 , Temperature 140 °C |
5950 psi @# of Cycles 100 , Temperature 284 °F |
R = 0.1, 8 Hz, dry | |
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A | |
1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A | |
3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 180/1A | |
Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
cond; ISO 179/1eU |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
cond; ISO 179/1eU | |
NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
dry; ISO 179/1eU | |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
dry; ISO 179/1eU | |
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA | |
1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA | |
3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | dry; ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | dry; ISO 11359-1/-2 |
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | dry; ISO 75-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | cond; IEC 60093 |
1.00e+15 ohm-cm | 1.00e+15 ohm-cm | dry; IEC 60093 | |
Dielectric Strength | 15.0 kV/mm | 381 kV/in | cond; IEC 60243-1 |
25.0 kV/mm | 635 kV/in | dry; IEC 60243-1 | |
Comparative Tracking Index | 400 V | 400 V | dry; IEC 60112 |