| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
| Radici Radilon® CST 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | 50mm/min; ASTM D638 |
| Reliance Industries Repol H020SU Polypropylene REPOL Polypropylene H020SU is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Global PP-1111-R Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | 50 mm/min; ISO 527-1,-2 |
| Inno-Comp INNOPOL® CS 1-3610 UW Polypropylene Homopolymer INNOPOL® CS 1-3610 UW is a white colored, flame retarded and UV-stabilized polypropylene homopolymer compound.INNOPOL® CS 1-3610 UW is recommended for producing electric articles by injection .. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | cond.; ISO 527-1, -2; 50 mm/min |
| Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Conditioned; ISO 527-1/-2 |
| Lanxess Durethan® B 35 FKA 000000 Nylon 6, Film Grade PA 6 Film grade, medium viscosity, nucleated, with processing and slip additives, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE co.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Conditioned; ISO 527-1/-2 |
| Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 50 mm/min; ASTM D638 |
| SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | SABIC - Japan Method |
| SABIC Innovative Plastics NORYL PX2795 PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1, 85 oC |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ISO 527-2 |
| Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ISO 527 |
| Unipetrol PP MONSTEN® GH 005 Polypropylene Homopolymer Made for injection molding. LTHA stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
| Tensile Strength, Yield | 35.0 MPa @Strain 300 % |
5080 psi @Strain 300 % |
ISO 527-1/-2 |
| Covestro Desmopan® DP 3055D Polyurethane injection molding gradewith high mechanical strength for articles subject to wearexcellent abrasion resistancegood wear resistancevery short cycle timesApplicationInjection molded engineering partsR.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | cond; ISO 527-1/-2 |
| DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | dry; ISO 527-1/-2 |
| EMS-Grivory Grivory® XE 4155 black 9992 PA612-I Information provided by EMS Grivory |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Aclo Accutech Polyethylene HD0234G20UVL High Density Glass Reinforced UV Stabilized |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Braskem H 203 Fiber Extrusion Polypropylene Homopolymer Continuous filaments for carpets, sewing yarns and ropes; Staple fibers for rugs and blankets; Nonwovens by thermobonded process.Information provided by Braskem. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
| Aclo Accutech Polypropylene Homopolymer HP0336T30L1 Talc Reinforced |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM-D638 |
| Braskem PD 943XP HOMO Polypropylene Homopolymer PD 943XP is a medium melt flow rate homopolymer with slip and antiblocking agents. It is suitable for blown film extrusion. This product features good impact strength, excellent gloss and transparen.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
| BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
| Tensile Strength, Yield | 35.0 MPa @Temperature 80.0 °C |
5080 psi @Temperature 176 °F |
ASTM Test |
| BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
| BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ISO 527-1/-2 |
| DSM Arnite® T06 206 T Impact Modified PBT (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
| Tensile Strength, Yield | 35.0 MPa @Temperature 23.0 °C |
5080 psi @Temperature 73.4 °F |
ISO 527 |
| DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | cond; ISO 527-1/-2 |
| DSM Akulon® K225-KV PA6 FR(30) Flame Retardant (Halogen free), Heat stabilized |
|||