Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carpenter 20-Mo6® Stainless Steel, Plate

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Carpenter 20-Mo6® Stainless Steel, Plate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, crevice corrosion and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. The alloy is designed for applications where better pitting and crevice-corrosion resistance are requires than 20Cb-3® stainless offers.20-Mo6® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 8.133 g/cc
0.2938 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 85
85
Tensile Strength, Ultimate 641 MPa
93000 psi
Tensile Strength, Yield 310 MPa
<br>@Strain 0.200 %
45000 psi
<br>@Strain 0.200 %
Elongation at Break 50 %
50 %
Reduction of Area 80 %
80 %
Modulus of Elasticity 186 GPa
27000 ksi
Poissons Ratio 0.29
0.29
Shear Modulus 72.1 GPa
10500 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 14.8 µm/m-°C
<br>@Temperature 25.0 - 100 °C
8.22 µin/in-°F
<br>@Temperature 77.0 - 212 °F
15.34 µm/m-°C
<br>@Temperature 25.0 - 300 °C
8.522 µin/in-°F
<br>@Temperature 77.0 - 572 °F
16.01 µm/m-°C
<br>@Temperature 25.0 - 500 °C
8.894 µin/in-°F
<br>@Temperature 77.0 - 932 °F
17.74 µm/m-°C
<br>@Temperature 25.0 - 900 °C
9.856 µin/in-°F
<br>@Temperature 77.0 - 1650 °F
Specific Heat Capacity 0.450 J/g-°C
0.108 BTU/lb-°F
Thermal Conductivity 12.1 W/m-K
<br>@Temperature 50.0 °C
84.0 BTU-in/hr-ft²-°F
<br>@Temperature 122 °F
14.8 W/m-K
<br>@Temperature 200 °C
103 BTU-in/hr-ft²-°F
<br>@Temperature 392 °F
18.2 W/m-K
<br>@Temperature 400 °C
126 BTU-in/hr-ft²-°F
<br>@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 22 - 26 %
22 - 26 %
Copper, Cu 2.0 - 4.0 %
2.0 - 4.0 %
Iron, Fe 31 %
31 %
as remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 5.0 - 6.7 %
5.0 - 6.7 %
Nickel, Ni 33 - 37 %
33 - 37 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001082 ohm-cm
0.0001082 ohm-cm
Copyright © lookpolymers.com All Rights Reserved