Chase Plastics CP Pryme® NN200L (DAM) Nylon 66, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN200L (DAM) Nylon 66, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.2 MPa
11200 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648