Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CTC SunPro® SP 200 P 5000 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer CTC (Composite Technologies)
Trade Name SunPro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC SunPro® SP 200 P 5000 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB500, CPN 4492Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
24Hr; ISO 294 3/4
Linear Mold Shrinkage, Transverse 0.0153 cm/cm
0.0153 in/in
24Hr; ISO 294 3/4
Melt Flow 15 - 25 g/10 min
15 - 25 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527-1/2
Flexural Modulus 0.750 GPa
109 ksi
0.05 in/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
Low Temp; ISO 180/1eA
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Front Barrel Temperature 204 - 216 °C
400 - 420 °F
Nozzle Temperature 204 - 216 °C
400 - 420 °F
Melt Temperature 204 - 227 °C
400 - 440 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
Descriptive Properties Value Comments
Boost Pressure (psi) 500-1500
Hold Pressure 50 - 75% of Boost
Screw Speed Medium to Fast