Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott KG4 Short Pass Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott KG4 Short Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG1, KG5
Physical Properties Metric English Comments
Density 2.53 g/cc
0.0914 lb/in³
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 613 °C
1140 °F
Optical Properties Metric English Comments
Refractive Index 1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
1.53

@Wavelength 365 nm
1.53

@Wavelength 365 nm
Hg
Transmission, Visible 47 %

@Wavelength 700 nm
47 %

@Wavelength 700 nm
85 %

@Wavelength 550 - 560 nm
85 %

@Wavelength 550 - 560 nm
Internal transmittance of 92% from 550-560 nm
IR Transmittance 77 %

@Wavelength 710 nm
77 %

@Wavelength 710 nm
Internal transmittance of 86% at 710 nm.
UV Transmittance <= 0.60 %

@Wavelength 200 - 290 nm
<= 0.60 %

@Wavelength 200 - 290 nm
86 %

@Wavelength 370 - 390 nm
86 %

@Wavelength 370 - 390 nm
Internal transmittance of 93-94% from 380-390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 2
2
Alkali Class, AR 3
3
Stain Resistance Class, FR 0.0
0.0