| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Ultramid® 1000-2 NF2001 PA66 (Conditioned).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | dry; ISO 1183 |
| Water Absorption | 8.5 % | 8.5 % | beginning dry; ISO 62 |
| Moisture Absorption at Equilibrium | 2.5 % | 2.5 % | beginning dry (23°C/50% R.H.); ISO 62 |
| Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM Data; MD |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50mm/min; ISO 527 |
| Elongation at Break | >= 50 % | >= 50 % | 50mm/min, Nominal strain; ISO 527 |
| Elongation at Yield | 25 % | 25 % | 50mm/min; ISO 527 |
| Tensile Modulus | 1.20 GPa | 174 ksi | 1mm/min; ISO 527 |
| Flexural Modulus | 1.10 GPa | 160 ksi | ISO Data |
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
| Charpy Impact Unnotched | NB | NB | ISO 179 |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179 | |
| Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179 |
| 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 257 °C | 495 °F | 10 K/min |
| 257 °C | 495 °F | ASTM Test |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural | |
| Commercial Status | Active America | |
| Impact Modified | No | |
| Primary Processing Technique | Injection Molding |