Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 160 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 1.10 GPa
160 ksi
STN EN ISO 178
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with..
Flexural Modulus 1.10 GPa
160 ksi
Tangent; ASTM D790
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.10 GPa
160 ksi
Tangent; ASTM D790
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.10 GPa
160 ksi
Tangent; ASTM D790
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
Flexural Modulus 1.10 GPa
160 ksi
Tangent; ASTM D790
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Network Polymers NPP 50-0158
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Flexural Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus >= 1.10 GPa
>= 160 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PP 8300K (EPT30R) Propylene and Ethylene Block Polymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade
Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application..
Flexural Modulus 1.10 GPa
160 ksi
Test 2
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
LyondellBasell Alathon® L5040TC High Density Polyethylene
ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and..
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Suzhou Hipro Polymers Hiprolon® 400 NN Nylon, conditioned
Hiprolon® 400 NN is a medium viscosity specialty polyamide. Features: low density, low water absorption, high dimension stability, high notched impact resistance in large temperature ranges, and..
Flexural Modulus 1.10 GPa
160 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b..
Flexural Modulus 1.10 GPa
160 ksi
At 2 mm/min; ISO 178
Borealis Daplen™ EE115T TPO Compound
Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th..
Flexural Modulus 1.10 GPa

@Strain <=0.400 %
160 ksi

@Strain <=0.400 %
ISO 178
Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin
Polyethylene: High molecular weight, high density fuel tank resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceGMP.PE.062 certification.Appl..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene
DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.10 GPa
160 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions such as corrugated board.Formolene 6501A is a medium impact copolymer with ..
Flexural Modulus 1.10 GPa
160 ksi
at 1% secant; ASTM D790
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin
DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Total PPR 12222 Random Copolymer Polypropylene
Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. It..
Flexural Modulus 1.10 GPa
160 ksi
0.05 in.min, tangent; ASTM D790
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Flexural Modulus 1.10 GPa
160 ksi
dry; ISO 178
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
ExxonMobil HDPE HMA 035 High Density Polyethylene Resin
Product Description: HMA 035 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, good impact strength and very high stiffness. Availability: Africa & Middle East, Asia ..
Flexural Modulus 1.10 GPa
160 ksi
1% secant; ASTM D790
Braskem CP 741 Blow Molding Polypropylene
Description: CP 741 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and general purpose additive package. CP 741 presents low odor/taste transfer, high mel..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Buckeye Polymers BP Flex D8020 UC85 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
Flexural Modulus 1.10 GPa
160 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Copyright © lookpolymers.com All Rights Reserved