Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Rovene® 6119 is a low glass transition temperature styrene-acrylic polymer that offers flexibility during movement of the substrate and water resistance. Rovene® 6119 also exhibits excellent tensile strength and maintains elongation properties when compounded with fillers.Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6119 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 51.5 - 52.5 %
51.5 - 52.5 %
Particle Size 0.20 µm
0.20 µm
pH 8.5 - 9.5
8.5 - 9.5
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
Descriptive Properties Value Comments
Emulsifiers Anionic