| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.26 g/cc | 0.0455 lb/in³ | Silicone Property; Arlon SQA-TMS-024 | 
| Thickness | 25.4 microns | 1.00 mil | Interleave | 
| 229 microns | 9.00 mil | Side 1; Arlon SQA-TMS-003 | |
| 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 | |
| 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 38 | 38 | Silicone Property; ASTM D2240 | 
| Tensile Strength | 6.96 MPa | 1010 psi | Silicone Property; ASTM D412 | 
| Elongation at Break | 579 % | 579 % | Silicone Property; ASTM D412 | 
| Tear Strength | 21.0 kN/m | 120 pli | [ppiw], Silicone Property; ASTM D624 | 
| Peel Strength | 2.73 kN/m | 15.6 pli | (S1 to S2) Bond Strength; Arlon SQA -TMS-011 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Dielectric Strength | 18.7 kV/mm | 475 kV/in | ASTM D149 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Cure Time |           120           min           @Temperature 204 °C  | 
                  2.00           hour           @Temperature 400 °F  | 
        Recommended Postcure Cycle | 
|           15.0           min           @Pressure 0.345 MPa, Temperature 177 °C  | 
                  0.250           hour           @Pressure 50.0 psi, Temperature 350 °F  | 
        Recommended Cure Cycle | |
| Shelf Life |           6.00           Month           @Temperature 21.1 °C  | 
                  6.00           Month           @Temperature 70.0 °F  | 
        From date of manufacture | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Color | Red | |
| Red | Substrate | |