| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
ND Industries StudGrade® 137 Permanent HT Threadlocker
General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required.
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Glastic GLASTHERM HT220 Insulation Sheet
Glastherm Grade HT220 is a thermal insulation sheet that is a highly heat-resistant material that combines low thermal conductivity with very high compressive strength at molding temperature. It is..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | Treatment Limit, Continuous |
|
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Master Bond Supreme 45HT Toughened Heat Resistant Two Component Epoxy Adhesive
Master Bond Polymer Supreme 45HT is a two component epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding and coating suitable f..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Loctite® 246 High Temperature/Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner
Design/Construction:Liner: Polyethylene Material: Fully Cured Silicone RubberProduct Use: Anti-Static Vacuum BaggingAppearance: Black elastomeric sheetThis data represents typical values for the pro..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 25122R060 0.060" (1.52 mm) Silicone Rubber on Laminated Fluoropolymer Film
Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 30400N125 0.125" (3.17 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Kodacel Carrier Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the production ma..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55949C028W 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 56596R065 0.065" (1.65 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon CP-475R Bulk Compound
Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R30960T030 0.030" (0.762 mm) Uncured Silicone Rubber with Kodacel Substrate
Design/Construction:Interleave: PolyethyleneAdd-on: Uncured Silicone Rubber Substrate: Kodacel CarrierAppearance: Translucent, high viscosity gum on release linersThis data represents typical values..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060)
Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 54B12R006 Silicone Rubber/Fiberglass Laminate
Cured silicone rubber with a fiberglass substrate.
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
3M 3615 General Purpose Glass Cloth Tape
3M™ Glass Cloth Tape 3615 is a general purpose, easy unwind tape coated with a silicone adhesive for many applications requiring high-temperature resistance, high adhesion, and a very strong, abras..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 32300R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
|
|||