| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 406 microns | 16.0 mil | |
| Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
| Thickness | 406 - 508 microns | 16.0 - 20.0 mil | Overall |
| Arlon 518581R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
| Thickness | 406 microns | 16.0 mil | |
| Hexcel® HexForce™ AGP370-5H Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
| Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
| Arlon 28540R015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1528 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for t.. |
|||
| Thickness | 406 microns | 16.0 mil | Layer 2; Arlon SQA-TMS-003 |
| Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be.. |
|||
| Thickness | 406 microns | 16.0 mil | substrate; Arlon SQA-TMS-003 |
| Arlon 56976B026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
| Thickness | 406 microns | 16.0 mil | Side 1; Arlon SQA-TMS-003 |
| Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
| Thickness | 406 microns | 16.0 mil | |
| 3M Scotch® 24 Electrical Shielding Tape Scotch® 24 Electrical Shielding Tape is an all-metal, open-weave, shielding braid tape in a flat, cable-like form. It is conformable due to the open-weave knit construction of two No. AWG tinned co.. |
|||
| Thickness | 406 microns | 16.0 mil | WFT |
| 3M Scotchkote™ FP 812 External Wall Coating 3M Scotchkote External Wall Coating FP 812 has been specifically developed as a low maintenance, high build coating for cemetitious and plaster wall surfaces.Information provided by 3M |
|||
| Thickness | 406 microns | 16.0 mil | Side 2; Arlon SQA-TMS-003 |
| Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
| Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
| Arlon 51250R016 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data should not be u.. |
|||
| Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
| Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
| Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
| Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
| Thickness | 406 microns | 16.0 mil | Prime Coated 1564 Fiberglass, Substrate |
| Arlon 56096R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56866R026 0.028" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil LDPEThis data represents typical values for the production mater.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
| Thickness | 406 microns | 16.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
| Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
| Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
| Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |
|||