| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 25.4 microns | 1.00 mil | Recommended |
|
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating
CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Backing |
|
Dielectric Polymers NT-7411-5 Fume Mask
(discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Good conformabilityChemical resistantApplications: For protecting large areas of printed circuit boards from splash and fumes duri..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Backing |
|
Dielectric Polymers NT-8511-2 Masking Tape
(discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityHigh temperature resistantApplications: For automotive and other masking ..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
Huntsman PE1903 EVA Film Extrusion
(discontinued **)
9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
LyondellBasell Montell 16502F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
LyondellBasell Montell 16502F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
Westlake Hifor SC74557 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc..
|
|||
| Thickness | 25.4 microns | 1.00 mil | as tested |
|
Total HL 428 HDPE Film Grade
Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro..
|
|||
| Thickness | 25.4 microns | 1.00 mil | ExxonMobil Method |
|
ExxonMobil Bicor™ 26MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
ExxonMobil EXACT™ 3139 Plastomer for Cast Film Applications
Product Description: Exact 3139 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3139 is designed for both monolayer and multilayer coe..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene
Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave |
|
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber
Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Liner |
|
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Facestock |
|
3M FM011 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave |
|
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave |
|
Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
|
|||
| Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
|
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
| Thickness | 25.4 microns | 1.00 mil | Adhesive |
|
3M 7122 Performance Paper Label Material
3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Polyester |
|
3M 7993MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave: Release liner to be determined (Temporarily FEP Film) |
|
Arlon R33670N004 0.004" (0.102 mm) Uncured Silicone Rubber with K2030 PEN Film Substrate
Design/Construction:Side 1: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inf..
|
|||
| Thickness | 25.4 microns | 1.00 mil | PET, Interleave |
|
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave |
|
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber
Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Interleave |
|
Arlon T3015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Facestock |
|
3M OFM0302 Outdoor UL Recognized White Polyester Label Product
3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ ..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE
(discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell..
|
|||
| Thickness | 25.4 microns | 1.00 mil | |
|
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for ..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Recommended |
|
Parker Chomerics CHO-SHIELD® 1091 Adhesion Promoter for Conductive Polyurethane Coatings
Information provided by Chomerics
|
|||
| Thickness | >= 25.4 microns | >= 1.00 mil | Side 1 |
|
Arlon 48571R006 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
|
|||
| Thickness | 25.4 microns | 1.00 mil | Side 1 |
|
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater..
|
|||