| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | Constant |
|
Plasma Coatings 20000 Surface Material
Information provided by Plasma Coatings
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | Shear Adhesive Failure (cohesive failure) |
|
Dielectric Polymers NT-702 Acrylic Tape
(discontinued **)
Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature s..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb
2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | Treatment Limit, Continuous |
|
Mid-Mountain Materials ARMATEX® SF22 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | Treatment Limit, Continuous |
|
Mid-Mountain Materials ARMATEX® SF37 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51581R015)
Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm)..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. ..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51571R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene Appearance: Black silicone gum on fiberglass clothThis da..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55579R043W 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 66211A007 0.007" (0.178 mm) Uncured Silicone Rubber Monofilament Polyester Fabric Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Monofilament Polyester Fabric Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represent..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon CP-375CR Silicone Rubber
bulk compound
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon CP-410XD Bulk Compound
Design/Construction:Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifica..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data ..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 49090R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51571R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum on fiberglass clothThis data Represents typical values for the production material. ..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51571XA015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum on fiberglass clothThis data Represents typical values for the production material. T..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe..
|
|||
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
|
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value..
|
|||