Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 635 microns Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 635 - 1270 microns
25.0 - 50.0 mil
Range of Thicknesses Available
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Thickness 635 - 1270 microns
25.0 - 50.0 mil
Range of Thicknesses Available
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&lt
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be ..
Thickness 635 microns
25.0 mil
Hexcel® HexForce™ 1507 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 635 microns
25.0 mil
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat..
Thickness 635 microns
25.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 19606R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: 0.003" PolyethyleneThis data represents typical values for the ..
Thickness 635 microns
25.0 mil
overall; Arlon SQA-TMS-003
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 635 microns
25.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
Thickness 635 microns
25.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
Thickness 635 microns
25.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material ..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber
Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..
Thickness 635 microns
25.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 31140R025 0.032" Uncured Silicone Rubber on Release Coated HDPE
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberRelease Carrier: Release Coated HDPEThis data represents typical values for the production material and should no..
Thickness 635 microns
25.0 mil
Silicone
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
Thickness 635 microns
25.0 mil
overall; Arlon SQA-TMS-003
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
Thickness >= 635 microns
>= 25.0 mil
Side 2
Arlon 51586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate..
Thickness 635 - 787 microns
25.0 - 31.0 mil
Overall
Arlon 55571R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic..
Thickness 635 microns
25.0 mil
Overall thickness
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and..
Thickness 635 microns
25.0 mil
Overall thickness
Arlon R31031R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1564 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for th..
Thickness 635 microns
25.0 mil
Silicone
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
Thickness 635 microns
25.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b..
Thickness 635 microns
25.0 mil
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
Copyright © lookpolymers.com All Rights Reserved