| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 635 - 1270 microns | 25.0 - 50.0 mil | Range of Thicknesses Available |
|
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
|
|||
| Thickness | 635 - 1270 microns | 25.0 - 50.0 mil | Range of Thicknesses Available |
|
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)<
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be ..
|
|||
| Thickness | 635 microns | 25.0 mil | |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo..
|
|||
| Thickness | 635 microns | 25.0 mil | |
|
Hexcel® HexForce™ 386 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
|
Arlon 19606R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: 0.003" PolyethyleneThis data represents typical values for the ..
|
|||
| Thickness | 635 microns | 25.0 mil | overall; Arlon SQA-TMS-003 |
|
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene
|
|||
| Thickness | 635 - 686 microns | 25.0 - 27.0 mil | Overall |
|
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Semi-Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications...
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 635 microns | 25.0 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
|
|||
| Thickness | 635 microns | 25.0 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
|
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material ..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber
Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..
|
|||
| Thickness | 635 microns | 25.0 mil | Silicone; Arlon SQA-TMS-003 |
|
Arlon 31140R025 0.032" Uncured Silicone Rubber on Release Coated HDPE
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberRelease Carrier: Release Coated HDPEThis data represents typical values for the production material and should no..
|
|||
| Thickness | 635 microns | 25.0 mil | overall; Arlon SQA-TMS-003 |
|
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
|
|||
| Thickness | >= 635 microns | >= 25.0 mil | Side 2 |
|
Arlon 51586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate..
|
|||
| Thickness | 635 - 787 microns | 25.0 - 31.0 mil | Overall |
|
Arlon 55571R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall thickness |
|
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall thickness |
|
Arlon R31031R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1564 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for th..
|
|||
| Thickness | 635 microns | 25.0 mil | Silicone |
|
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Thickness | 635 microns | 25.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
|
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b..
|
|||
| Thickness | 635 microns | 25.0 mil | |
|
Zircar Zirconia ZYW-30A Zirconia Cloth Insulation