Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene, Interleave
165 microns
6.50 mil
Side 1
165 microns
6.50 mil
Side 2
457 microns
18.0 mil
Prime Coated 162 Fiberglass, Substrate
762 microns
30.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
Compound Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Elongation at Break >= 300 %
>= 300 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 177 °C
0.500 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month
6.00 Month
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 31.7 - 37.7
Uncoated Fabric Break Strength 420 lb/in
Fill Direction, Substrate Property
700 lb/in
Warp Direction, Substrate Property