ExxonMobil Escorene® LD-612 EVA Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-612 EVA Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This resin can also be considered for blending with homopolymer resins to improve their toughness.Applications: Large injection molded shapes.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50, Condition C; ASTM D1693
Melt Flow 2.1 g/10 min
2.1 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 33
33
ASTM D2240
Tensile Strength, Ultimate 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D638
Elongation at Break 1300 %
1300 %
ASTM D638
Flexural Modulus 0.140 GPa
20.3 ksi
1% Secant, ASTM D790
Tensile Impact Strength 2.50 kJ/m²
1.19 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
Exxon Method