Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier  (discontinued *
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Tensile Strength 5.52 MPa
800 psi
Compound Property; ASTM D412
Arlon R36772R008 0.008" (0.203 mm) Fully Cured, Unsupported, Silicone Rubber with Fiberglass Substrate  (
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material ..
Tensile Strength >= 5.52 MPa
>= 800 psi
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2564 is a smooth fini..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 51570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 51586X015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 56106R026 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 56590R026 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data Represents typical values fo..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 56596R065 0.065" (1.65 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon CP-368 Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Tensile Strength >= 5.52 MPa
>= 800 psi
Silicone Property
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should ..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 31140R025 0.032" Uncured Silicone Rubber on Release Coated HDPE
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberRelease Carrier: Release Coated HDPEThis data represents typical values for the production material and should no..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 44576B009A 0.0085" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or ..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia..
Tensile Strength 5.52 MPa
800 psi
Layer 2, Silicone Property; ASTM D412
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon R33706R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri..
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..