| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 74 | 74 | Conditioned; ISO 868 |
| 83 | 83 | ISO 868 | |
| Tensile Strength at Break | 85.0 MPa | 12300 psi | Conditioned; ISO R 527 |
| 145 MPa | 21000 psi | ISO R 527 | |
| Elongation at Yield | 3.0 % | 3.0 % | ISO R 527 |
| 5.0 % | 5.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 3.40 GPa | 493 ksi | Conditioned; ISO 178 |
| 5.60 GPa | 812 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1A |
| 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/IeU |
| 5.00 J/cm² | 23.8 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/IeA |
| 1.10 J/cm² | 5.23 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 35.0 µm/m-°C | 19.4 µin/in-°F | ASTM E831 |
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
| 33.0 kV/mm | 838 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |