| Zhejiang Juner 201-G0 Flame Resistant Nonreinforced |
Polybutylene Terephthalate (PBT) |
|
| Zhejiang Juner 201-G20 20% Glass Fibre Reinforced |
Polybutylene Terephthalate (PBT) |
|
| Zhejiang Juner 201-G30 30% Glass Fibre Reinforced |
Polybutylene Terephthalate (PBT) |
|
| Zhejiang Juner 301-G0 Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 301-G20 20% Glass Fibre Reinforced and Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 301-G30 30% Glass Fibre Reinforced and Flammable Resistant |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 302-G0 Flammable Resistant and Low Separate Out Mode |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 302-G20 20% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode |
Polyethylene Terephthalate (PET) |
|
| Zhejiang Juner JEPP2007 PP For Automotive Parts |
Polypropylene, Molded |
|
| Zhejiang Juner JEPP2056 PP For Automotive Parts |
Polypropylene, Molded |
|
| Zhejiang Juner JEPP263 Weatherability PP Series |
Polypropylene, Molded |
|
| Zhejiang Juner JEPPA003 High Glossy PP |
Polypropylene, Molded |
|
| Zhejiang Juner JEPPB003 High Glossy PP |
Polypropylene, Molded |
|
| Zhejiang Juner JEPPB005 High Glossy PP |
Polypropylene, Molded |
|
| Zhejiang Juner JEPPB006 High Glossy PP |
Polypropylene, Molded |
|
| Zhejiang Juner JEPPBC001 Weatherability PP Series |
Polypropylene, Molded |
|
| Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA-A1 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6 |
Nylon 6 |
|
| Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6 |
Nylon 6 |
|
| Zhejiang Juner PA-A6 GF20% |
Nylon 6, 20% Glass Fiber Filled |
|
| Zhejiang Juner PA-A6-1 MF25% |
Nylon 6, 20% Mineral Filled |
|
| Zhejiang Juner PA-A6-3 GF/MF Reinforced |
Nylon 6, Glass/Mineral Reinforced |
|
| Zhejiang Juner PA-A6-4 Non-Reinforced |
Nylon 6, Unreinforced |
|
| Zhejiang Juner PA-A6-66H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Zhejiang Juner PC Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Zhejiang Juner PC/ABS Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Zhejiang Juner PC-A1 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A2-1 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A2-10 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A2-9 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A2-9A Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A5 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A6-2 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A7 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A7-5 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A7-7 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PP201-G30 PP For Automotive Parts |
Polypropylene, Molded |
|
| Zhejiang Juner PP430R Weatherability PP Series |
Polypropylene, Molded |
|
| Zhejiang Juner PP6-1JE PP For Automotive Parts |
Polypropylene, Molded |
|
| Zhejiang Juner PP8 PP For Automotive Parts |
Polypropylene, Molded |
|
| Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC/PBT Alloy |
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced |
|
| Zhejiang Juner PC/PET Alloy |
Polycarbonate/PET Polyester Blend |
|
| Zhejiang Juner PC-3-1 Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Zhejiang Juner PC-A1-1 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-10 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-11 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-11B Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-3 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-33 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-7 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-9 Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PC-A1-9A Top-Grade Flame Retardant UV-Resistant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide |
Nylon 6, Mineral Reinforced, Impact Grade |
|
| Zhejiang Juner PC/ABSz-4 Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|