| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) | 
| Manufacturer | Zhejiang Juner New Materials Co. | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Zhejiang Juner PC-3-1 Alloy.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.21 g/cc | 0.0437 lb/in³ | GB/1033 | 
| Water Absorption | 0.30 % | 0.30 % | GB/T1034 | 
| Linear Mold Shrinkage | 0.0050 - 0.0060 cm/cm | 0.0050 - 0.0060 in/in | GB/15585 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | GB/1040 | 
| Flexural Strength | 82.0 MPa | 11900 psi | GB/9341 | 
| Charpy Impact Unnotched | NB | NB | IS0179-1:2000 | 
| Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | IS0179-1:2000 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | GB/1634 | 
| Flammability, UL94 | HB - V-0 | HB - V-0 | GB/T2408 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | D257 | 
| Comparative Tracking Index | 200 V | 200 V | GB/4207 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
| Drying Temperature | 100           °C @Time 14400 sec | 212           °F @Time 4.00 hour | Chute Hot-Wind | 
| 100           °C @Time 18000 sec | 212           °F @Time 5.00 hour | Horizontal Oven | |
| Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Chromatism (?E) | =0.8 | |
| Granule Diameter | Φ3x3-5 | |
| Speed of Shoot, % | 35-80 | |
| Surface Polish | High | |
| Weatherability | Adjustive |