Material Notes:
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, Frameworks of Deflection Coils, Hi-Pressure Outputs Package, Plugs of Kinescopes Autos and Others: Ignition Systems, Heating Systems, Electricity Distribution Systems, Tail Lights Base, Shells of Ignition Coils, Door Handles, Air-Condition LatticesInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
D792
Water Absorption 0.090 %
0.090 %
23°C•24h; D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 115 MPa
16700 psi
D638
Elongation at Break 4.0 %
4.0 %
D638
Flexural Strength 180 MPa
26100 psi
D790
Flexural Modulus 8.00 GPa
1160 ksi
D790
Charpy Impact Unnotched 4.80 J/cm²
22.8 ft-lb/in²
IS0179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
IS0179
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
D696
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
D257
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
D150
Dielectric Strength 21.0 kV/mm
533 kV/in
D149
Dissipation Factor 0.025

@Frequency 1e+6 Hz
0.025

@Frequency 1e+6 Hz
D150
Processing Properties Metric English Comments
Processing Temperature 255 - 265 °C
491 - 509 °F
Nozzle Temperature 245 °C
473 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 130 - 140 °C

@Time 14400 sec
266 - 284 °F

@Time 4.00 hour
Injection Pressure 80.0 - 120 MPa
11600 - 17400 psi
3-15 sec
Back Pressure 8.00 - 18.0 MPa
1160 - 2610 psi