| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Zhejiang Juner New Materials Co. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.54 g/cc | 0.0556 lb/in³ | GB/1033 |
| Water Absorption | 0.60 % | 0.60 % | 23°C•24h |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 70.0 MPa | 10200 psi | GB/1040 |
| Flexural Strength | 115 MPa | 16700 psi | GB/9341 |
| Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | IS0179-1:2000 |
| Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179-1:2000 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | GB1634 |
| Flammability, UL94 | V-0 | V-0 | GB/T2408 |
| Flammability Test | 30 | 30 | Flame Remainder (%); GB/9345 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 375 V | 375 V | GB/4207 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 225 - 260 °C | 437 - 500 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 110 °C @Time 7200 sec |
230 °F @Time 2.00 hour |
Vacuum Pressure, -0.08 MPa |
| 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
Chute Hot-Wind | |
| 120 °C @Time 21600 sec |
248 °F @Time 6.00 hour |
Horizontal Oven | |
| Injection Pressure | 40.0 - 90.0 MPa | 5800 - 13100 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Speed of Shoot, % | 35-90 |