Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, Frameworks of Deflection Coils, Hi-Pressure Outputs Package, Plugs of Kinescopes Autos and Others: Ignition Systems, Heating Systems, Electricity Distribution Systems, Tail Lights Base, Shells of Ignition Coils, Door Handles, Air-Condition LatticesInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
D792
Water Absorption 0.080 %
0.080 %
23°C•24h; D570
Linear Mold Shrinkage 0.0040 - 0.0090 cm/cm
0.0040 - 0.0090 in/in
D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
D638
Elongation at Break 3.0 %
3.0 %
D638
Flexural Strength 160 MPa
23200 psi
D790
Flexural Modulus 7.00 GPa
1020 ksi
D790
Charpy Impact Unnotched 3.80 J/cm²
18.1 ft-lb/in²
IS0179
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
IS0179
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
D696
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
D257
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
D150
Dielectric Strength 20.0 kV/mm
508 kV/in
D149
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
D150