Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
GB/1033
Water Absorption 0.60 %
0.60 %
23°C•24h
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
GB/1040
Flexural Strength 115 MPa
16700 psi
GB/9341
Charpy Impact Unnotched 2.80 J/cm²
13.3 ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
GB1634
Flammability, UL94 V-0
V-0
GB/T2408
Flammability Test 30
30
Flame Remainder (%); GB/9345
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
350 V
GB/4207
Processing Properties Metric English Comments
Processing Temperature 225 - 255 °C
437 - 491 °F
Mold Temperature 40.0 - 100 °C
104 - 212 °F
Drying Temperature 110 °C

@Time 7200 sec
230 °F

@Time 2.00 hour
Vacuum Pressure, -0.08 MPa
120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Chute Hot-Wind
120 °C

@Time 21600 sec
248 °F

@Time 6.00 hour
Horizontal Oven
Injection Pressure 40.0 - 90.0 MPa
5800 - 13100 psi
Descriptive Properties Value Comments
Speed of Shoot, % 30-80