| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Zhejiang Juner New Materials Co. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Zhejiang Juner PC Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.21 g/cc | 0.0437 lb/in³ | GB/1033 |
| Water Absorption | 0.30 % | 0.30 % | GB/T1034 |
| Linear Mold Shrinkage | 0.0050 - 0.0060 cm/cm | 0.0050 - 0.0060 in/in | GB/15585 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 52.0 MPa | 7540 psi | GB/1040 |
| Flexural Strength | 82.0 MPa | 11900 psi | GB/9341 |
| Charpy Impact Unnotched | NB | NB | IS0179-1:2000 |
| Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | IS0179-1:2000 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | GB/1634 |
| Flammability, UL94 | HB - V-0 | HB - V-0 | GB/T2408 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | D257 |
| Comparative Tracking Index | 200 V | 200 V | GB/4207 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
| Drying Temperature | 100 °C @Time 14400 sec |
212 °F @Time 4.00 hour |
Chute Hot-Wind |
| 100 °C @Time 18000 sec |
212 °F @Time 5.00 hour |
Horizontal Oven | |
| Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chromatism (?E) | =0.8 | |
| Granule Diameter | Φ3x3-5 | |
| Speed of Shoot, % | 35-80 | |
| Surface Polish | High | |
| Weatherability | Adjustive |