Zhejiang Juner PP6-1JE PP For Automotive Parts

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PP6-1JE PP For Automotive Parts.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
GB/1033
Linear Mold Shrinkage 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
GB/15585
Melt Flow 1.1 - 1.4 g/10 min
1.1 - 1.4 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
GB/1040
Flexural Strength 48.0 MPa
6960 psi
GB/9341
Charpy Impact Unnotched 0.500 J/cm²
2.38 ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
GB1634
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
D257
Processing Properties Metric English Comments
Processing Temperature 170 - 230 °C
338 - 446 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-85