Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150 Synthetic Rubber (Compound)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150B Synthetic Rubber (Compound)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150L Synthetic Rubber (Compound)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR230 Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR303 Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR406 Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR412 Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR617 Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR617 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UPILEX 75S (75 micron) Polyimide Film
Polyimide, Thermoset Film
UPILEX
UBE UPILEX VT Polyimide Film
Polyimide, Thermoset Film
UPILEX
UBE UPIMOL® R Polyimide Shape
Polyimide, TS
UPIMOL®
UBE UPIMOL® S High Heat Polyimide Shape
Polyimide, TS
UPIMOL®
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR153A Oil-Extended Synthetic Rubber (Raw Polymer)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR230 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UBEPOL VCR617 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Rubber or Thermoset Elastomer (TSE)
UBEPOL
UBE UPILEX 25S (25 micron) Polyimide Film
Polyimide, Thermoset Film
UPILEX
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape
Polyimide, TS
UPIMOL®
UBE UPIMOL® SA201 Heat-Resistant Polyimide Shape