Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 14.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm
356 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm
356 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Dielectric Strength 14.0 kV/mm
356 kV/in
ASTM D149
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Dielectric Strength 14.0 kV/mm
356 kV/in
Short Time; ASTM D149
Plenco 51240 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers.
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Powder grades for masterbatches.Information provided by Solvay Specialty Polymers.
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion..
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm
356 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
Dielectric Strength 14.0 kV/mm
356 kV/in
ASTM D149
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Dielectric Strength 14.0 kV/mm
356 kV/in
GB/T1408.1-2006
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD
Dielectric Strength 14.0 kV/mm
356 kV/in
GB/T1408.1-2006
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm
356 kV/in
ASTM D149-95a
Thermoseal KLINGERSIL® C-4401 General Application Gasketing
Synthetic FiberNitrile BinderExcellent SealabilityExcellent Chemical ResistanceGood Creep RelaxationGeneral Purpose SheetData for this material is available for download into ANSYS xml format: C4401..
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm

@Thickness 3.00 mm
356 kV/in

@Thickness 0.118 in
IEC 60243
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Dielectric Strength 14.0 - 17.0 kV/mm
356 - 432 kV/in
Average value: 15.2 kV/mm Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, step-by-step. ASTM D149
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI..
Dielectric Strength 14.0 kV/mm

@Thickness 3.00 mm
356 kV/in

@Thickness 0.118 in
ASTM D149
Sumitomo Bakelite North America RX® 655 Novolac Phenolic
Fiberglass and mineral reinforced phenolic molding compound with very high fill level (75%). Excellent dimensional stability and good strength at elevated temperatures. Very low thermal expansion ..
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, Step by Step
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Dielectric Strength 14.0 kV/mm
356 kV/in
Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6
18% crystallinity. Information supplied by Elastomer Engineering.
Dielectric Strength 14.0 kV/mm
356 kV/in
ASTM D149
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..