| Category | Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , ECTFE Fluoropolymer |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.68 g/cc | 1.68 g/cc | ASTM D792 |
| Water Absorption at Saturation | <= 0.10 % | <= 0.10 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
| Melt Flow | 18 g/10 min <br>@Load 2.16 kg,<br> Temperature 275 °C |
18 g/10 min <br>@Load 4.76 lb,<br> Temperature 527 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 90 | 90 | R-Scale; ASTM D785 |
| Hardness, Shore D | 75 | 75 | ASTM D2240 |
| Tensile Strength at Break | 47.0 MPa <br>@Temperature 23.0 °C |
6820 psi <br>@Temperature 73.4 °F |
50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 30.0 MPa <br>@Temperature 23.0 °C |
4350 psi <br>@Temperature 73.4 °F |
50 mm/min; ASTM D638 |
| Elongation at Break | 250 % <br>@Temperature 23.0 °C |
250 % <br>@Temperature 73.4 °F |
50 mm/min; ASTM D638 |
| Elongation at Yield | 5.0 % <br>@Temperature 23.0 °C |
5.0 % <br>@Temperature 73.4 °F |
50 mm/min; ASTM D638 |
| Tensile Modulus | 1.66 GPa <br>@Temperature 23.0 °C |
241 ksi <br>@Temperature 73.4 °F |
50 mm/min; ASTM D638 |
| Flexural Strength | 47.0 MPa <br>@Temperature 23.0 °C |
6820 psi <br>@Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
| Flexural Modulus | 1.69 GPa <br>@Temperature 23.0 °C |
245 ksi <br>@Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
| Izod Impact, Notched | 2.10 J/cm <br>@Thickness 3.20 mm,<br> Temperature -40.0 °C |
3.93 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -40.0 °F |
ASTM D256 |
| NB <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
NB <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 | |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | vs. Itself; ASTM D1894 |
| Coefficient of Friction, Static | 0.20 | 0.20 | vs. Itself; ASTM D1894 |
| Taber Abrasion, mg/1000 Cycles | 5.0 <br>@Load 0.500 kg |
5.0 <br>@Load 1.10 lb |
CS-17 Wheel |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 40.0 J/g | 17.2 BTU/lb | Crystallization Heat; ASTM D3418 |
| 42.0 J/g | 18.1 BTU/lb | ASTM D3418 | |
| CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
| Specific Heat Capacity | 0.962 J/g-°C <br>@Temperature 23.0 °C |
0.230 BTU/lb-°F <br>@Temperature 73.4 °F |
ASTM D3418 |
| Thermal Conductivity | 0.150 W/m-K <br>@Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F <br>@Temperature 104 °F |
ASTM C177 |
| Melting Point | 242 °C | 468 °F | ASTM D3418 |
| Crystallization Temperature | 222 °C | 432 °F | Peak, DSC; ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ASTM D648 |
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746A |
| Glass Transition Temp, Tg | 85.0 °C | 185 °F | DMA |
| Decomposition Temperature | 405 °C | 761 °F | 1% mass loss, N2; TGA |
| Flammability, UL94 | V-0 | V-0 | UL 94 |
| Oxygen Index | 52 % | 52 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 5.50e+16 ohm-cm <br>@Temperature 23.0 °C |
5.50e+16 ohm-cm <br>@Temperature 73.4 °F |
50% RH; ASTM D257 |
| Dielectric Constant | 2.57 <br>@Frequency 1.00e+6 Hz,<br> Temperature 23.0 °C |
2.57 <br>@Frequency 1.00e+6 Hz,<br> Temperature 73.4 °F |
ASTM D150 |
| Dielectric Strength | 14.0 kV/mm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
356 kV/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D149 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Features | Low Viscosity | |
| Forms | Powder | |
| Generic | ECTFE | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Uses | Masterbatch | |
| Wire & Cable Applications |