Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 955 PC Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | |
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | PLC code 4; UL 746A |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL PX1265 PPE+PS Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | PLC code 4; UL 746A |
SABIC Innovative Plastics Noryl 731H PPE+PS High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min @Thickness 3.00 mm |
>= 5.91 in/min @Thickness 0.118 in |
UL Rating PLC 4 (>150 mm/min.) |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 945 PC (Asia Pacific) Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |