| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific)
Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa..
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Lexan® 925 PC
Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa..
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Lexan® FL900 PC
Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i..
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | |
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics ULTEM CRS5201 PEI
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics ULTEM CRS5301 PEI
30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 4521 PBT
VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 457 PBT
6.5% GR PBT, UL94 V-0/5V.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | PLC code 4; UL 746A |
|
SABIC Innovative Plastics Valox® CS860 PBT+PET (Asia Pacific)
30% glass reinforced PBT+PET blend. Color stable, FR. Housewares, appliances; iron skirt, oven trim/panels.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS
LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses).
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 451E PBT
20% GR. Easy flow version of VALOX 451.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific)
20% GR. Easy flow version of VALOX 451.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
|
|||
| High Voltage Arc-Tracking Rate, HVTR |
>=
150
mm/min <br>@Thickness 3.00 mm
|
>=
5.91
in/min <br>@Thickness 0.118 in
|
UL Rating PLC 4 (>150 mm/min.) |
|
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe..
|
|||
| High Voltage Arc-Tracking Rate, HVTR |
>=
150
mm/min <br>@Thickness 3.00 mm
|
>=
5.91
in/min <br>@Thickness 0.118 in
|
UL Rating PLC 4 (>150 mm/min.) |
|
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL FN170X PPE+PS
Foamable resin. All properties at 10% density reduction; 0.250"" thick test specimens.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL FN215X PPE+PS
Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction.
|
|||
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
|
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..
|
|||