Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 0.750 - 0.820 mm |
15 - 30 sec @Thickness 0.0295 - 0.0323 in |
|
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Valox® DR48 PBT 17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 3.00 mm |
15 - 30 sec @Thickness 0.118 in |
UL Rating PLC 3 (15-30 sec) |
Covestro Bayblend® T 84 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL Rating PLC 3 (15-30 sec) |
Covestro Makrolon® 2605 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content. |