LG Chemical 92HR SAN Resin

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LG Chemical 92HR SAN Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter cases, toothbrushes, and cassette tape cases
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 3.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
32 g/10 min

@Load 10.0 kg,
Temperature 220 °C
32 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength, Yield 77.0 MPa
11200 psi
50 mm/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
50 mm/min; ASTM D638
Modulus of Elasticity 3.21 GPa
466 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 128 MPa
18600 psi
50 mm/min; ASTM D790
Flexural Modulus 3.71 GPa
538 ksi
15 mm/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C

@Thickness 6.35 mm
196 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 107 °C
225 °F
1000 g; ASTM D1525
Flammability, UL94 HB
HB
1/8 in
HB
HB
1/16 in
Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
UL Rating PLC 5 (120-180 sec)
Comparative Tracking Index 400 - 600 V
400 - 600 V
UL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min
<= 0.394 in/min