Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
Conditioned; ASTM D149 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.18 mm |
533 kV/in @Thickness 0.125 in |
Conditioned; ASTM D149 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.18 mm |
533 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
|
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 3.20 mm |
533 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.1%); ASTM-D149 |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 1.25%); ASTM-D149 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 1.0%); ASTM-D149 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 1.4%); ASTM-D149 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
continuous tension; ASTM D149-75 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
continuous tension; ASTM D149-75 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |