Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 575 V Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 583 V Grade Count:6 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Comparative Tracking Index | 200 - 600 V | 200 - 600 V | Average value: 473 V Grade Count:65 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 572 V Grade Count:14 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Comparative Tracking Index | 225 - 600 V | 225 - 600 V | Average value: 477 V Grade Count:68 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Comparative Tracking Index | 225 - 600 V | 225 - 600 V | Average value: 479 V Grade Count:68 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Comparative Tracking Index | 300 - 600 V | 300 - 600 V | Average value: 524 V Grade Count:28 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Comparative Tracking Index | 375 - 600 V | 375 - 600 V | Average value: 436 V Grade Count:14 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | IEC 60112 |
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | IEC 60112 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical MI-750 MIPS Medium impact |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | ASTM UL746A |
Kuraray Genestarâ„¢ GT2330 Nylon, 33% Glass Filled Toughness V-0 Grade. It is well suited for components requiring a high strength in pin fitting process, due to high ductility properties. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical 25SPI GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | PLC 1; UL 746 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 750 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 575 V Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 593 V Grade Count:5 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 583 V Grade Count:3 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | Average value: 575 V Grade Count:4 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Comparative Tracking Index | 350 - 600 V | 350 - 600 V | Average value: 552 V Grade Count:52 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | Solution A; IEC 60112 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Comparative Tracking Index | 175 - 600 V | 175 - 600 V | Average value: 304 V Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |