| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
| Comparative Tracking Index | 350 V | 350 V | |
| Radici Radiflam® S RV300AE (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
| Comparative Tracking Index | 350 - 599 V | 350 - 599 V | Average value: 464 V Grade Count:6 |
| Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| SABIC Innovative Plastics Lexan® BFL2000U PC Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Cond)
(discontinue The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
| Comparative Tracking Index | 350 - 600 V | 350 - 600 V | Average value: 493 V Grade Count:7 |
| Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
| Comparative Tracking Index | 350 - 600 V | 350 - 600 V | Average value: 549 V Grade Count:28 |
| Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Lanxess Pocan® B 3225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Lanxess Pocan® B 3235 901510 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Lanxess Pocan® DP 1105 000000 PBT PBT, non-reinforced, injection molding, extrusion, improved flowability |
|||
| Comparative Tracking Index | 350 V | 350 V | A solution |
| LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
| Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
| SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East) NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications. |
|||
| Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
| SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
| Comparative Tracking Index | 350 V | 350 V | Solution A; IEC 60112 |
| Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding... |
|||
| Comparative Tracking Index | 350 V | 350 V | TS EN 60112 |
| Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960.. |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Covestro Bayblend® FR 3006 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradehigh heat resistanceVicat/B 120 = 110 °Ceasy flowUL-listing 94 V-1 at 1.5 mm and V-0 at 2.0 mmPreprocessingMax. Water content |
|||
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
| Comparative Tracking Index | 350 V | 350 V | |
| Covestro Bayblend® KU 2-1500 Polycarbonate/ABS Blend Flame retardant extrusion grade.Applications: Bulky parts for DT-copying machines.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and official.. |
|||
| Comparative Tracking Index | 350 V | 350 V | dry; IEC 60112 |
| DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
| Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
| Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
| Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
| Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
| Comparative Tracking Index | >= 350 V | >= 350 V | Solution A; IEC 60112 |
| Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered Information provided by Eurotec® |
|||
| Comparative Tracking Index | 350 V | 350 V | Solution B; IEC 60112 |
| Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |
|||