Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093:1980-01 |
Nylacast POM C Acetal Copolymer The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IPC-TM-650.2.5.17 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 93 |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | dry; IEC 60093 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(d The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 5.05e+14 ohm Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY ZF3021 PPE+PS (Europe-Africa-Middle East) LNP* STAT-LOY* ZF3021 is a compound based on PPE + PS Blend resin containing Glass Fiber. Added features include Antistatic, Flame Retardant. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Styrolution Luran® S 778 TE UV Colored ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding Good surface finish Nylon 6/6.6 alloy for injection molding.Information provided by Polyram. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC 93 |
Total PS CPDS 815 High Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | DIN 53482 |
Polyram PlusTek PB801 Nylon 6, Impact Modified impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | DIN 53482 |
Polyram PlusTek PD100 Nylon 12, Injection Molding Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 GR45 NL HS PA6, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |