Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Surface Resistance | 1000 - 1.00e+15 ohm | 1000 - 1.00e+15 ohm | Average value: 4.02e+14 ohm Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.64e+14 ohm Grade Count:35 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1000 - 1.00e+15 ohm | 1000 - 1.00e+15 ohm | Average value: 4.25e+14 ohm Grade Count:12 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.70e+14 ohm Grade Count:11 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | Average value: 6.79e+14 ohm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Surface Resistance | 4.00 - 1.00e+15 ohm | 4.00 - 1.00e+15 ohm | Average value: 8.00e+14 ohm Grade Count:5 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Surface Resistance | 12.0 - 1.00e+15 ohm | 12.0 - 1.00e+15 ohm | Average value: 8.00e+14 ohm Grade Count:15 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 3.35e+14 ohm Grade Count:6 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 2.41e+14 ohm Grade Count:12 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.67e+14 ohm Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 4.88e+13 ohm Grade Count:23 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.59e+14 ohm Grade Count:24 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+15 ohm | 1.00e+6 - 1.00e+15 ohm | Average value: 4.05e+13 ohm Grade Count:30 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+15 ohm | 1.00e+12 - 1.00e+15 ohm | Average value: 6.40e+13 ohm Grade Count:19 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 4.06e+14 ohm Grade Count:9 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Surface Resistance | 100 - 1.00e+15 ohm | 100 - 1.00e+15 ohm | Average value: 1.11e+14 ohm Grade Count:9 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 5.05e+14 ohm Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 2.57e+14 ohm Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.70e+14 ohm Grade Count:6 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | Average value: 2.50e+14 ohm Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.09e+14 ohm Grade Count:21 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Surface Resistance | 3000 - 1.00e+15 ohm | 3000 - 1.00e+15 ohm | Average value: 1.35e+14 ohm Grade Count:23 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+15 ohm @Temperature 200 - 200 °C |
1.00e+15 - 1.00e+15 ohm @Temperature 392 - 392 °F |
Average value: 1.00e+15 ohm Grade Count:2 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |